80 Hours operation of a tubular solid oxide fuel cell using propane/air
Yu Chen,Minyi Lu,Huazheng Yang,Yingbang Yao,Tao Tao,Shengguo Lu,Chao Wang,Rajendran Ramesh,Michaela Kendall,Kevin Kendall,Xiaoping Ouyang,Bo Liang
DOI: https://doi.org/10.1016/j.apenergy.2020.115099
IF: 11.2
2020-08-01
Applied Energy
Abstract:<p>High power density and simple design are vital for these fuel cell-based portable power generation devices. This study provides an 8.6 g tubular SOFC with embedded a catalytic partial oxidation reformer, which is fabricated and operated for more than 100 h using propane/air. Nickel-iron nanosheets, as catalysts for reforming, supported on α-Al<sub>2</sub>O<sub>3</sub> foam ceramic are synthesized by hydrothermal treatment. Testing for 80 h gives a power degradation of about 20% compared with the initial value. It is mainly attributed to sulfur-poisoning of nickel near anode/electrolyte interface according to transmission electron microscope (TEM) analysis. From TEM/energy dispersive spectroscopy line-scan results across the anode/electrolyte interface, sulfur as either aggregate at the nickel/yttria-stabilized zirconia grain boundaries or on the nickel grain surface, and no obvious carbon phase is founded. The maximum power density is 0.67 W cm<sup>−2</sup> at 700 °C using propane/air (12 vol% propane), about 5% higher than the same cell using 20 vol% hydrogen.</p>
energy & fuels,engineering, chemical