Ultrafine-grained W-based alloys prepared by HIP with ultrahigh hardness and excellent thermal stability
Zaoming Wu,Lin He,Linsen Ye,Xiaofeng Yang,Jiajia Zhang,Hongbo Lei
DOI: https://doi.org/10.1016/j.ijrmhm.2023.106318
IF: 4.804
2023-09-01
International Journal of Refractory Metals and Hard Materials
Abstract:Pure W with grain size of 1.77 μm, ultrafine-grained W-10wt.%Cr-2wt.%Ti (W-10 C-2 T) alloy with grain size of 161 nm and W-10wt.%Cr-4wt.%Ti (W-10 C-4 T) alloy with grain size of 148 nm, were prepared by mechanical alloying followed by hot isostatic pressing (HIP) sintering. Ultrafine-grained structure stability mechanisms of W-10 C-2 T and W-10 C-4 T can be mainly ascribed to the thermodynamic aspect illustrated by the kinetic calculation of critical maximum W grain size. The average grain size of W-10 C-4 T is smaller than that of W-10 C-2 T, and the increasing additional amount of Ti can further inhibits grain growth. The second phase particles can interact with free oxygen to purify and strengthen grain boundaries, and the faster thermal diffusion rate of Cr and Ti can improve the density of W-10 C-2 T and W-10 C-4 T alloys obviously, compared with pure W. The Vickers hardness of W-10 C-2 T and W-10 C-4 T alloys were tested, and results show that they possess ultrahigh hardness, the value of their Vickers hardness is 1237 ± 74 kgf/mm2 and 1402 ± 46 kgf/mm2, respectively, which is much larger than that of pure W and coarse-grained W-based alloys. The ultrahigh hardness comes from the abundant grain boundaries (GBs) that act as obstacles and potential barriers for dislocation motion, and second phase strengthening. High-temperature annealing treatment results show that W-10 C-2 T and W-10 C-4 T alloys possess excellent thermal stability at the annealing temperature of 1000 °C and 1100 °C, and the thermal stability mechanisms were explored.
materials science, multidisciplinary,metallurgy & metallurgical engineering