Interfacial Microstructure and Mechanical Property of the Discontinuous Short Tungsten Fiber-Reinforced Tungsten Matrix Composites

C. Chen,Y. Chen,K. L. Li,S. Wang,Y. F. Zhang,Y. R. Mao,Jan W. Coenen,J. Wang,L. M. Luo,Y. C. Wu
DOI: https://doi.org/10.1016/j.matchar.2024.114214
IF: 4.537
2024-01-01
Materials Characterization
Abstract:For tungsten fiber-reinforced tungsten matrix (Wf/W) f /W) composites, the interface between W matrix and W fiber has a dominant effect on the mechanical properties. In this study, the interfacial microstructure in the Wf/W f /W composites with or without Y2O3 2 O 3 coating deposited on W fiber is investigated. The crystal structure of the Y2O3 2 O 3 coating composed of nano-sized columnar grains on the W fibers is cubic. And the crystal structure of Y2O3 2 O 3 coating changes to be face centered cubic after sintering in the Wf/W f /W composites. Two kinds of interfaces, including the interface between W matrix and Y2O3 2 O 3 coating, the interface between W fiber and Y2O3 2 O 3 coating, are present in the Wf/W f /W composites. Different orientation relationships are observed in these two kinds of interface. The stable orientation relationship with (111 ) Y 2 O 3 // (011 ) W have the lowest interfacial energy. The Y2O3 2 O 3 interface is essential for improving the toughening behavior of Wf/W f /W composites and impeding the abnormal grain growth on the surface of W fiber sintering at low temperature. The recrystallization nucleus is developed by the bonding between W powder and W fiber during sintering, and then grow fast into W fiber. The apparent activation energy of abnormal grain growth of W fibers is about 242.7 KJ/mol sintering at temperature between 1500 and 1800 degrees C. The abnormal large grains usually show intergranular brittle fracture and make the W fiber be brittle.
What problem does this paper attempt to address?