Factors Influencing the Burn-Out Rate of Fujian Anthracite Coal in CFB Boilers

HE Hong-zhou,LUO Zhong-yang,CEN Ke-fa
DOI: https://doi.org/10.3321/j.issn:1000-6761.2006.03.013
2006-01-01
Abstract:Coal quality and the boiler's operational condition are the main factors that influence the burn-out rate of Fujian anthracite coal.Due to coal quality and combustion characteristics such as compactness of interior particle structure,poor reactivity and strong fragmentation tendency at high temperatures are the main intrinsic factors that cause Fujian anthracite coal hard to burn out in CFB boilers;whereas boiler operation factors such as the distribution of coal granules fed,excess air ratio,secondary air rate,as well as the way of its feeding,and the combustion temperature have also a great effect on the coal's burn-out rate.Test results show that coarser sieved particles with a narrow size range,increased excess air ratio and the secondary air rate,enhanced secondary air's stirring and penetrating capability and increased combustion temperature all help to raise the burn out rate of Fujian anthracite in CFB boilers.The excess air ratio should be kept within(1.25)-(1.30),and combustion temperature raised to about 1000 °C to obtain better combustion effect.Figs 8,tables 2 and refs 15.
What problem does this paper attempt to address?