Interface microstructure and mechanical properties of the brazed SiO2 glass ceramic and 30Cr3 high-tensile steel joint

L.X. Zhang,L.Z. Wu,datong liu,J.C. Feng,H.B. Liu
DOI: https://doi.org/10.1016/j.msea.2008.05.050
2008-01-01
Abstract:In this study, a commercially available Ag–Cu–Ti braze alloy foil was used to join SiO2 glass ceramic and 30Cr3 high-tensile steel. According to experimental observations, the interface structure can be expressed as SiO2 glass ceramic/TiSi2+Ti4O7/Ti2Cu+Cu3Ti3O/Ag(s.s)+Cu(s.s)/TiFe2/30Cr3 high-tensile from SiO2 glass ceramic side to 30Cr3 high-tensile steel side. With the increased brazing temperature, the thickness of Ti2Cu+Cu3Ti3O layer increases at first and then reduces. The thickness of TiSi2+Ti4O7 layer and that of TiFe2 layer rise with the increased brazing temperature. According to experimental results of the mechanical properties, the maximum shear strength is 37MPa when the joint was brazed at 900°C for 5min.
What problem does this paper attempt to address?