Continuous Sic(Oal) Fiber from Polymer Precursor
YX Yu,XD Li,F Cao,CM Zheng,YD Wang,J Wang
DOI: https://doi.org/10.3321/j.issn:1002-185x.2006.04.038
2006-01-01
Abstract:Continuous SiC(OAl) fibers, named KD-A fibers, were prepared by the melt-spinning of ceramic precursor polyalumino-carbosilane, air-curing, and pyrolizing at 1300 degrees C. These fibers contain small amount of aluminum and 7wt% oxygen. The fibers are characterized by chemical analysis, tensile strength test, scanning electron microscope, atomic force microscope, high resolution transmission electron microscope, X-ray diffraction. The tensile strength, Young's modulus and diameter of the KD-A fiber are 2.6 GPa, 210 GPa, 12 mu m similar to 14 mu m, respectively. The KD-A fibers have higher thermal stability, more excellent oxidation resistance than the Nicalon fibers. The properties of the KD-A fibers have reached the level of Hi-Nicalon fibers.