Abstract:In this paper, a new method for preparing ultrafine tungsten-molybdenum composite powders has been proposed. The carbothermic pre-reduction of the mixture of molybdenum trioxide and tungsten trioxide with insufficient carbon black under argon atmosphere was carried out, to generate the pre-reduced tungsten-molybdenum composite powder containing a small amount of residual dioxide. Thereafter, the obtained reaction product was subjected to hydrogen reduction to remove the residual dioxide and generate pure tungsten-molybdenum composite powder with the particle size of 100–200 nm. Two kinds of ultrafine tungsten-molybdenum alloy powders (Mo-30 wt% W, Mo-70 wt% W) were prepared. The residual carbon of the finally obtained product was about 0.01–0.02 wt% after the hydrogen reduction. The sintering behavior of ultrafine W–Mo powders and the properties of sintered samples are investigated. After sintering ultrafine Mo-30 wt% W and Mo-70 wt% W powders at 1600 °C, the relative density of the sintered compacts was about 99%, 97%, and the microhardness were 287 HV and 350 HV, respectively. Meanwhile, as increasing the sintering temperature from 1200 to 1600 °C, the relative density and microhardness of the compacts gradually increased.
materials science, multidisciplinary,metallurgy & metallurgical engineering
What problem does this paper attempt to address?