Abstract:AbstractThe 0‐3 type CaBi4Ti4O15:30 wt%BiFeO3 composite shows much better high‐temperature piezoelectric properties than the single‐phase CaBi4Ti4O15 or BiFeO3 ceramics. The composite with 0‐3 type connectivity exhibits a high density of 7.01 g/cm3, a saturated polarization of 21.5 μC/cm2 and an enhanced piezoelectric d33 of 25 pC/N. After the poled composite was annealed at 600°C, its d33 is 21 pC/N at room temperature. Resistance of the composite decreases slowly from 109 ohm at 20°C to ~105 ohm at 500°C. Furthermore, the poled composite shows strong radial and thickness dielectric resonances at 20°C‐500°C.