High Piezoelectric D33 Coefficient of Lead-Free (ba0.93ca0.07)(ti0.95zr0.05)o3 Ceramics Sintered at Optimal Temperature

Wei Li,Zhijun Xu,Ruiqing Chu,Peng Fu,Guozhong Zang
DOI: https://doi.org/10.1016/j.mseb.2010.09.003
2011-01-01
Abstract:Lead-free (Ba0.93Ca0.07)(Ti0.95Zr0.05)O3 (BCZT) ceramics were prepared using a solid-state reaction technique. The structure and electrical properties were investigated with a special emphasis on the influence of sintering temperature. Crystalline structures and microstructures were analyzed by X-ray diffraction and scanning electron microscope (SEM) at room temperature. The BCZT ceramics sintered at 1450°C show the highest densification and exhibit excellent piezoelectric properties of high piezoelectric coefficient d33=387pC/N, planar mode electromechanical coupling coefficient kp=44.2%, mechanical quality factor Qm=140 and Curie temperature Tc=108°C.