High heat flux test and post examination of ITER divertor W/Cu monoblock mock-ups

Zhao-xuan SUN,Qiang LI,Wan-jing WANG,Ji-chao WANG,Xing-li WANG,Ran WEI,Chun-yi XIE,Guang-nan LUO
DOI: https://doi.org/10.16568/j.0254-6086.201704013
2017-01-01
Abstract:High heat flux test of ITER divertor W/Cu monoblock mock-ups were finished. All tested mock-ups successfully withstood the heat cycles above and met the requirements of high heat flux performances specified by IO. After HHF test, the post analysis was performed on tested mock-ups. The results found the debonding of the Cu/CuCrZr interface and the crack of W. The scanning electron microscope (SEM) image of the break shows that intergranular rupture was the main mechanism of the W crack. The recrystallization was observed in the W monoblocks and the recrystallized depth was estimated by metallography analysis. The temperature distribution was also obtained by finite element analysis and a good correspondence with recrystallization observed by experiment was found.
What problem does this paper attempt to address?