Manufacturing and testing of ITER FW CuCrZr/316L(N)-IG explosive Bi-metallic plates

Qian LI,Ji-hong WU,Dan-hua LIU,Ping-huai WANG,Zong-qin LI,Rui MA,Ji-ming CHEN
DOI: https://doi.org/10.16568/j.0254-6086.201601007
2016-01-01
Abstract:CuCrZr/316L(N)-IG explosion bi-metallic plate manufactured by CuCrZr plate and 316L(N)-IG plate was used as heat sink component of ITER first wall (FW). CuCrZr plate and 316L(N)-IG plate were used as base plate and flyer plate, respectively. Metallographic test, hardness test and tensile test were performed. It turns out that there is an obvious wavy microstructure on the interface of CuCrZr/316L(N)-IG with mean wave length of 1200μm and mean wave height of 500μm. The tensile strength is up to 394MPa at room temperature. Six FW mockups were made, and it turned out that the bi-metallic plate met ITER requirement.