Tungsten Wires and Porous NiAl Prepared Through Directional Solidification and Selective Dissolution

Zhilong Zhao,Jianjun Gao,Lufeng Wei,Kai Chui
DOI: https://doi.org/10.1080/10426914.2017.1303146
IF: 4.7832
2017-01-01
Materials and Manufacturing Processes
Abstract:The combination of directional solidification and selective dissolution was applied to fabricate tungsten (W) wires and porous NiAl matrix. A NiAl-W pseudobinary eutectic alloy with 1.5at.% tungsten was directionally solidified in a Bridgman-type oven at 1700 degrees C. Results confirmed that the relationships of the growth rate with the interfibrous spacing and diameter of W fibrous phases in the directionally solidified samples are in accordance with the Jackson and Hunt (J-H) model. Afterward, the NiAl matrix was selectively dissolved in an HCl:H2O2 solution to reveal W wires, which present various three-dimensional (3D) morphologies at different growth rates. The W fibrous phases in the NiAl-W alloy samples were then selectively removed with a mixed etchant of ammonium acetate to form a porous NiAl matrix at a constant potential. Dynamic corrosion curves revealed that etching W from the NiAl matrix was inhibited after 2-3h. The porous structures of NiAl after removing W phases are linked to the 3D morphologies of W fibrous phases embedded in the NiAl matrix. The aspect ratio of W wires and the structures of porous NiAl can be adjusted by selecting the process parameters of this combined technology.
What problem does this paper attempt to address?