Studies on the Sample Preparation and Mediate Temperature Isothermal Tempering Process for Austenite with Homogeneous Nitrogen Content

卑多慧,胡明娟,朱祖昌,潘健生
DOI: https://doi.org/10.3969/j.issn.1001-3814.2003.03.004
2003-01-01
Abstract:The 225℃ tempering process and the corresponding microhardness of supersaturated Fe-(2.6~2.7)wt% N austenite were studied.Fe-(2.6~2.7)wt%N austenite could be prepared by two-step nitriding at 640℃.It was found that γ′-Fe 4N phase was firstly precipitated from γ-Fe(N) and α-Fe phase was then present after 1~2 h of tempering when tempered at 225℃.The γ-Fe(N) decomposed slowly in the first 3 h, comparatively,however,the rate of γ-Fe(N) decomposition increased so rapidly in the following half an hour that the parent phase of super-saturated austenite could mostly transformed into two-phase strutures α-Fe+γ′-Fe 4N.The γ-Fe(N) disappeared completely after 8~10 h tempering.The coarse of decomposed products was not evident even after long tempering.As a result,the microhardness of tempering products of γ-Fe(N) could exceed above 1000 HV0.025 after 8~15 h tempering and then decreased a little with the tempering time,but could still keep above 900 HV0.025 even after 25 h of tempering treatment.The more nitrogen content the austenite contained,the sooner the decomposition processed and the higher the microhardness of the decomposed products presented.
What problem does this paper attempt to address?