Influence of Ni Content on the Structure and Mechanical Properties of Ultrafine WC-Ni-VC-TaC Hardmetals

Rong Huiyong,Peng Zhijian,Ren Xiaoyong,Wang Chengbiao,Fu Zhiqiang,Qi Longhao,Miao Hezhuo
2011-01-01
Rare Metal Materials and Engineering
Abstract:A series of ultrafine WC-Ni hardmetals with different fractions of nickel metal binder from 6-10 wt% were fabricated by sparking plasma sintering with the assistance of VC and TaC as inhibitors of WC grain growth. The results indicate that the WC grain size of the as-prepared WC-Ni-VC-TaC hardmetals is in the range of 0.2-0.4 gm; there are lots of micro-pores in the materials, and their sizes are decreased with increasing content of Ni in the hardmetals. With the increase of Ni content in the hardmetals, the relative density of the as-prepared hardmetals is decreased first and then increased, and their hardness is decreased from 24500 MPa to 18600 MPa (HV1), but the flexural strength is increased from 1600 MPa to 2140 MPa.