Investigation Of Size Effect On The Giant Dielectric Cacu3ti4o12 Ceramic

Kai Chen,Wei Li,Yifei Liu,Peng Bao,Xiaomei Lu,Jinsong Zhu
DOI: https://doi.org/10.1080/10584580490898344
2004-01-01
Integrated Ferroelectrics
Abstract:CaCu3Ti4O12 ceramics were prepared by conventional solid-state reaction with different sintering temperature. Impedance spectroscopy on CaCus Ti4O12 ceramics demonstrates that they are electrically heterogeneous and C06 (sintered in air at 1060degreesC) is the most suitable for the device application. Surface observation and analysis of the grain-boundary-grained structure were proceeded by use of scan electronic microscopy, which confirms that the samples have surely different crystal grain sizes and C06 has bigger grain size of about 20 mum. The mechanical relaxation spectroscopy on C06 was also performed and a mechanical loss peak was found, which was attributed to the thermally activated behaviors of some units immanent in grains.