Structural and magnetic properties of Fe73.5Cu1Nb3−xTixSi13.5B9 (x≤3) alloys

Mi Yan,Hui Tong,Shan Tao,Junhu Liu
DOI: https://doi.org/10.1016/j.jallcom.2010.06.042
IF: 6.2
2010-01-01
Journal of Alloys and Compounds
Abstract:Fe73.5Cu1Nb3−xTixSi13.5B9 (x=0, 1, 2, 3) amorphous ribbons were prepared by melt spinning technique, then subjected to isothermal treatments for 1h at 500 and 550°C, respectively. Differential scanning calorimetry (DSC) measurements show that the α-Fe(Si) phase can be formed over a wider temperature with the increase of Ti content, from 156°C for x=0 to 164°C for x=3. Volume fraction of nanocrystalline α-Fe(Si) phase also increases with the increase of Ti content after annealing at 500 and 550°C for 1h, which is beneficial to enhance the ferromagnetic exchanging coupling in the alloys. DO3 ordered superstructure phase formed in the samples with Ti content of 2% and 3%. Better soft magnetic properties were obtained after annealing for 1h at 550°C than at 500°C, accompanied by the enhancement of saturation magnetization from 140.68emu/g for x=0 to 148.87emu/g for x=3 and the reduction of coercivity from 3.194G for x=0 to 1.151G for x=3.
What problem does this paper attempt to address?