Preparation of Core-Shell Silicon/Porous Carbon Powders

Shi Li-min,Zhao Hong-sheng,Yan Ying-hui,Tang Chun-he
DOI: https://doi.org/10.1016/j.carbon.2009.09.026
IF: 5.7
2009-01-01
New Carbon Materials
Abstract:Core-shell silicon/porous carbon powders were fabricated by coating silicon powders with phenolic resin, followed by carbonization at 800 degrees C for 2 h. The influence of phenolic resin volume percent, silicon mass percent and aging temperature on the formation of silicon/phenolic resin precursor powders was investigated. The resulting powders were characterized by X-Ray diffraction and scanning electron microscopy The optimum conditions for the formation of silicon/phenolic resin precursor powders are found to be: volume ratio of phenolic resin to alcohol, < 1; mass ratio of Si to alcohol, < 2; and aging temperature, at 30-60 degrees C. The resin carbon shell of the resulting powders is formed by the pyrolysis of phenolic resin during carbonization treatment and the carbon content in the core-shell silicon/porous carbon increases with the content of phenolic resin in precursor powders. The large amount of gas produced in the pyrolysis process creates pores in the carbon shell.
What problem does this paper attempt to address?