Effects of Molding Temperature on Properties of Porous SiC Ceramics

YANG Yang,ZHAO Hong-sheng,LIU Zhong-guo,ZHANG Kai-hong,LI Zi-qiang
DOI: https://doi.org/10.3969/j.issn.1001-4381.2011.05.013
2011-01-01
Abstract:The core-shell structure precursor powders were synthesized through coat mix process,and a small amount of Al2O3,SiO2 and Y2O3 composite additives was added.A series of porous silicon carbide ceramics were produced after molding,carbonization and sintering.The porosity,density,thermal expansion coefficient,bending strength and thermal shock resistance of porous silicon carbide ceramics were analyzed.The results show that the porous silicon carbide ceramic with molding temperature 80℃ possesses best general performance.When the molding temperature is very low,the barium phenolic resin coated over the core-shell structure precursor powders can not flow adequately,leading a loose structure and lower strength for the final porous silicon carbide ceramic.While the phenolic resin flows too much with excessive high molding temperature,some of composite additives are coated by phenolic resin and can not touch each other adequately,thereby the effect of composite additive is weaken.
What problem does this paper attempt to address?