Preparation and Properties of Cacu3ti4o12 Thick Film by Aerosol Deposition Method

Ji-Feng Ma,Yuan-Hua Lin,Ce-Wen Nan,Takaaki Tsurumi
DOI: https://doi.org/10.4028/www.scientific.net/kem.368-372.126
2008-01-01
Key Engineering Materials
Abstract:CaCu3Ti4O12 (CCTO) ceramic thick films have been prepared on Copper substrate, using ceramic powders by an aerosol deposition method (ADM). The ceramic powders are prepared by traditional solid state reaction processing at 1100 oC for 5 h. X-ray diffraction and scanning electron microscopy are used to investigate the microstructure and the phase composition of the deposited films. The results indicate that thick films are pure CCTO phase and homogenous. The dielectric impedance spectra indicate that the dielectric constant of CCTO thick film can reach 3×103.