Abstract:Niobium powder was fabricated by sodiothermic reduction process using K2NbF7 as a raw materials, KCl and KF as the diluents and sodium as a reducing agent. The apparatus for the experiment was designed and built specifically for the present study. Varying properties of niobium powder depending on reaction temperature and excess of reducing agent were analyzed. The niobium particle size increased significantly as reduction temperature increased from 993 to 1093K. The particle size was fairly uniform at given reaction temperature, varying from 0.2μm to 50nm depending on the reaction temperature. The yield of niobium powder increased from 58% to 83% with a increase in reaction temperature. The average particle size of niobium powder was improved from 70nm to 0.2μm with increase in the amount of sodium excess. In addition, the yield of niobium powder was 82% in the 5% sodium excess.
materials science, multidisciplinary,metallurgy & metallurgical engineering
What problem does this paper attempt to address?