THE MANUFACTURING OF NIOBIUM POWDER BY HUNTER PROCESS

JAE-SIK YOON
DOI: https://doi.org/10.1142/s0218625x10013898
2010-04-01
Surface Review and Letters
Abstract:Niobium powder was fabricated by metallothermic reduction process using K 2 NbF 7 as the raw material, KCl and KF as the diluents and Na as the reducing agent. The apparatus for the experiment was designed and built specifically for the present study. Varying properties of niobium powder depending on reaction temperature and excess of reducing agent were analyzed. The niobium particle size increased significantly as the reduction temperature increased from 993 to 1093 K. The particle size was fairly uniform at a given reaction temperature, varying from 0.2 μ m to 50 nm depending on the reaction temperature. The yield of niobium powder increased from 58 to 83% with an increase in reaction temperature. The average particle size of niobium powder was improved from 70 nm to 0.2 μ m with the increase in the amount of Na excess. In addition, the yield rate of Nb powder was 82% in the 5% excess sodium.
chemistry, physical,physics, condensed matter
What problem does this paper attempt to address?