Low Carbon and Deep-bed Sintering Practice of Laiwu Steel's 265m~2 Sinter Machine

Ma Qing-guo
Abstract:In order to actualize low carbon and deep-bed sintering in the No.4 265 m2 sinter machine,Laiwu Steel took a series of measures such as segregation distribution,preheating sinter mixture by steam,applying punching device on the surface of material bed,strengthening mini-pelletized sintering and low-temperature sintering processes,adopting ZTM sintering machine head and tail seals and new double discharging valve.Then the material thickness reached between 750 mm and 780 mm.The solid fuel consumption was reduced from 55.27 kg/t to 49.32 kg/t.
Engineering,Materials Science