Abstract:<p>In this study, magnetic properties and microstructure of <em>L</em>1<sub>0</sub> MnGa thin films deposited at different substrate temperatures (<em>T</em><sub>s</sub>) were carried out in order to determine the onset of the hard magnetic MnGa phase onto glass substrate. The thickness of MnGa thin film was kept at 200 nm while the <em>T</em><sub>s</sub> was varied from room temperature (RT) to 600°C. When the <em>T</em><sub>s</sub> was below 300℃, only Mn phases with small grain size were observable. However, the further increase in <em>T</em><sub>s</sub> to 325℃ led to the appearance of <em>L</em>1<sub>0</sub> (111) peak indicating the presence of the hard magnetic phase in the film on the glass substrate. Also, the continuous rise in <em>T</em><sub>s</sub> enhanced the magnetic properties such as saturation magnetization (<em>M</em><sub>s</sub>) and coercivity (<em>H</em><sub>c</sub>). The crystal size of <em>L</em>1<sub>0</sub> MnGa phase and surface roughness of the film were also increased with the increase of <em>T</em><sub>s</sub>. The selected area diffraction pattern (SADP) of Transition Electron Microscopy (TEM) effectively identified that the coexistence of pure Mn and <em>A</em>1 MnGa phases were present at <em>T</em><sub>s</sub> &lt; 300℃ and that the <em>L</em>1<sub>0</sub> MnGa started to appear at <em>T</em><sub>s</sub> = 325℃ while the completion of <em>L</em>1<sub>0</sub> MnGa phase was seen at <em>T</em><sub>s</sub> &gt; 400℃. The High-Resolution TEM (HRTEM) images revealed the lattice and amorphous regions present in the MnGa thin film at <em>T</em><sub>s</sub> = 325℃. Nevertheless, an increase of <em>T</em><sub>s</sub> to 600℃ presented a wide range of <em>L</em>1<sub>0</sub> (111) lattice signifying the thin film is still in MnGa phase. The onset of hard magnetic <em>L</em>1<sub>0</sub> MnGa phase is found out to be at 325℃.</p>
materials science, multidisciplinary,physics, condensed matter
What problem does this paper attempt to address?