Preparation and Characterization of Self-Lubricating CaF2@ZrO2/YSZ Composite Coating

Zeng, Xian
DOI: https://doi.org/10.1007/s11666-022-01424-x
IF: 2.839
2022-06-25
Journal of Thermal Spray Technology
Abstract:Core-shell CaF 2 @ZrO 2 powders were prepared by sol method combined with centrifugal atomization drying, aiming at preventing CaF 2 from burning during the APS deposition of YSZ-based abradable seal coating. The microstructure, chemical composition, hardness and wear behavior of the YSZ coating, the YSZ-10CaF 2 coating and the YSZ-10CaF 2 @ZrO 2 coating were comparatively investigated. The results suggested that the core-shell powders effectively protected CaF 2 , where the amount of CaF 2 remained in the YSZ-10CaF 2 @ZrO 2 coating was higher than that in the YSZ-10CaF 2 coating. The YSZ coating had the highest average hardness of 97.3 HR45Y and exhibited a mixed wear mechanism of adhesive and fatigue wear with a friction coefficient of 0.23 and a volume wear rate of 7.28 mm 3 /N m. Contributed to soft and self-lubricating CaF 2 , the hardness of the YSZ-10CaF 2 and YSZ-10CaF 2 @ZrO 2 coatings slightly declined to 95.1 and 94.5 HR45Y correspondingly. The YSZ-10CaF 2 coating showed a mixed wear mechanism of abrasive and fatigue wear with a friction coefficient of 0.14 and a volume wear rate of 4.67 mm 3 /N m. Moreover, the YSZ-10CaF 2 @ZrO 2 coatings showed a mixed wear mechanism of reduced adhesive and fatigue wear with a friction coefficient of 0.10 and a volume wear rate of 2.66 mm 3 /N m.
materials science, coatings & films
What problem does this paper attempt to address?