Fracture behaviour of Hastelloy X elaborated by laser powder bed fusion: influence of microstructure and building direction

B. Vieille,A. Duchaussoy,S. Benmabrouk,R. Henry,C. Keller
DOI: https://doi.org/10.1016/j.jallcom.2022.165570
IF: 6.2
2022-05-28
Journal of Alloys and Compounds
Abstract:Laser Power Bed Fusion (LPBF) results in complex meso and microstructures, which significantly change the fracture mechanisms of Hastelloy X superalloys. This article aims to investigate the role played by original crack orientation (perpendicular or co-linear to sample lasing planes) on the fracture toughness values of LPBF HX. Single notched three-point bending samples were manufactured vertically (V) or horizontally (H) to estimate the fracture toughness for these two original crack directions. The highest value (about 1360 kJ/m2) is computed in V specimens with an original crack parallel to the lasing plane whereas a value of 1042 kJ/m2 is estimated in H specimens with the second crack orientation. Compared to the values obtained in cast specimens, the fracture toughness of LPBF specimens is virtually 5 to 6 times higher. A non-self-similar cracking is specific to V specimens revealing a more tortuous crack path than in H specimens with self-similar cracking. In both cases, ductile failure is driven by both transgranular and intergranular modes. Nevertheless, the strong morphological texture contributes to promote intragranular fracture mode in V specimens which requires more energy than the one dissipated by an intergranular failure associated to H samples. Consequently, the fracture toughness is significantly higher in V specimens.
materials science, multidisciplinary,chemistry, physical,metallurgy & metallurgical engineering
What problem does this paper attempt to address?