Non-metallic Inclusion Evolution in a Liquid Third-Generation Advanced High-Strength Steel in Contact with Double-Saturated Slag

Dai Tang,Petrus Christiaan Pistorius
DOI: https://doi.org/10.1007/s11663-021-02084-y
2021-02-16
Metallurgical and Materials Transactions B
Abstract:<p class="a-plus-plus">Slag doubly saturated with CaO and MgO was used to investigate slag–steel–inclusion reactions for a third-generation advanced high-strength steel with an intermediate level of alloying elements (6 pct Mn, 1.5 pct Al and 1.5 pct Si). The change in oxide inclusion composition was Al<sub class="a-plus-plus">2</sub>O<sub class="a-plus-plus">3</sub> → spinel → MgO, as in Al-killed steels. No MnO or SiO<sub class="a-plus-plus">2</sub> was detected in the inclusions. (Mg, Mn)S sulfide inclusions apparently formed during solidification.</p>