Abstract:Kaolinite as an aluminum-rich clay mineral is widely distributed in kaolin, coal gangue and mill tailings, etc. Herein, alumina extraction from the low-grade kaolin was explored via multi-stage hydrothermal process in the presence of NaOH and lime. In single stage, maximum alumina leaching ratio was found to be 33.64% in the presence of 20 g/L NaOH, 180 ? leaching temperature, 2 h leaching time and CaO/SiO2 molar ratio of 0.7. The formation of zeolites due to limited solubility of aluminate ions resulted in the low alumina leaching ratio. Then, a multi-stage hydrothermal process was proposed to improve the alumina leaching, with each stage being carried out at 180 ? for 0.1 h. The cumulative alumina leaching ratio attained 72.09% after three-stage hydrothermal process; after desilication, the lixivium was used for preparing pseudo-boehmite via carbonation. Conclusively, the multi-stage hydrothermal process achieved the efficient extraction of alumina from kaolinite and presented great potential in improving the economic value of low-grade kaolin.
What problem does this paper attempt to address?