Microwave Dielectric Properties of Low-Temperature Sintered Ca[(Li<sub>1/3</sub>Nb<sub>2/3</sub>)<sub>0.95</sub>Zr<sub>0.05</sub>]O<sub>3−δ</sub>−0.04TiO<sub>2</sub> Ceramics

Hui Xiong,Gang Xiong,Cui Hua She
DOI: https://doi.org/10.4028/www.scientific.net/amr.535-537.832
2012-01-01
Advanced Materials Research
Abstract:The effects of B2O3 on the sinterability and microwave dielectric properties of Ca[(Li1/3Nb2/3)0.95Zr0.05]O3−δ−0.04TiO2 (CLNZ−0.04TiO2) ceramics were investigated . B2O3 doping can effectively reduce sintering temperatue by 150~200°C. The temperature coefficient of resonator frequency τf increased with an increase of B2O3 content and sintering temperatue. When B2O3 of 2wt% were added, the optimum microwave dielectric properties: εr =31.8,Qf =17240GHz and τf = − 5.9×10−6/°C were obtained at the sintering temperature of 950°C.