Improved Strength in Wrought Mg–Y–Ni Alloys by Adjusting the Block-Shaped LPSO Phase and Plate-Shaped Γ′ Phase

S. Z. Wu,X. G. Qiao,S. H. Qin,Y. Q. Chi,M. Y. Zheng
DOI: https://doi.org/10.1016/j.msea.2021.142198
2022-01-01
Abstract:The microstructure and mechanical properties of two Mg-Y-Ni alloys with different volume fraction of blockshaped LPSO phase and different number densities of plate-shaped gamma' phase were investigated. The volume fraction of block-shaped LPSO phase increases with the content of Y and Ni in the Mg-Y-Ni alloys with Y/Ni atomic ratio of 1. The plate-shaped gamma' phase is formed in the matrix of the as-cast alloys and grows across the matrix during the preheating before extrusion, and its number density increases with increasing content of Y and Ni. After extrusion, the block-shaped LPSO phase is distributed along extrusion direction, and the plate-shaped gamma' phase can be observed in both non-dynamic recrystallized (non-DRXed) grains with strong basal texture and dynamic recrystallized (DRXed) grains with random texture. The increased volume fraction of LPSO phase improves the tensile yield strength of the as-extruded Mg-Y-Ni alloys, accompanied by the decrease in ductility. In addition to the obvious strengthening from the LPSO phase, the plate-shaped gamma' phase is also an effective strengthening phase which can hinder the movement of the slip systems in non-DRXed and DRXed grains of the Mg-Y-Ni alloys. The Mg94Y3Ni3 (at%) alloy containing the highest volume fraction of block-shaped LPSO phase and the highest number density of plate-shaped gamma' phase exhibits the superior tensile yield strength of 502 MPa after extrusion.
What problem does this paper attempt to address?