Abstract:•Bi2O3 with 0.10 mol % contents doped into B2O3-ZnO (99:1) to manufacture the glass powder at 550 °C.•TGA illustrates that the AgI is well retained in the samples at 450 °C.•The whole immobilized route is simple by glass-powder without considering the complex phase changing.•The leaking rate of iodine is 1.89–3.40 × 10−5 g∙m−2∙d−1 for 7 days, which shows considerable chemical durability.