Research on Tribology Property of Si-3N-4 Ceramic and Chilled Iron under Oil-Less Lubrication

XIANG Zhong-xia,DONG Gang,SHEN Zhao-guang,LIN Bin
DOI: https://doi.org/10.3785/j.issn.1006-754x.2005.05.014
2005-01-01
Journal of Engineering Design
Abstract:A series of tests on friction and wear of Si_3N_4 ceramic and chilled iron under oil-less lubrication were conducted on MG-200 Friction Wear Machine by adopting block-on-disc wear test method,during which the values of wear rate and friction coefficient of Si_3N_4 ceramic and chilled iron were achieved.Additionally the friction and wear behaviors were analyzed through SME images and percentage of different chemical elements distributed on friction surface.The result indicated wear rates of Si_3N_4 ceramic and friction coefficient between Si_3N_4 ceramic and chilled iron under oil-less lubrication are much less than wear rates and friction coefficient under dry friction condition.Wear rate of Si_3N_4 ceramic rose with the increase of loads between Si_3N_4 ceramic and chilled iron while the effect of relative sliding speed on wear rate of Si_3N_4 ceramic is not as significant as that of load.For the friction coefficient between Si_3N_4 ceramic and chilled iron,it decreased with the increase of relative sliding speed and the change on load had little influence on it.Wear of Si_3N_4 ceramic was caused by interaction of chemical wear,abrading wear and particle's peeling off,among which the chemical one was dominant.
What problem does this paper attempt to address?