Study on the Ash Deposition Propensity and Mechanism of Shenhua Coal

ZHOU Jun-hu,ZHAO Xiao-hui,YANG Wei-juan,CAO Xin-yu,LIU Jian-zhong,CEN Ke-fa
DOI: https://doi.org/10.3321/j.issn:0258-8013.2007.08.007
2007-01-01
Abstract:Shenhua coal is one of the high quality power coals which has large reserves and high calorific value.But for its low ash fusion temperatures,those boilers burning Shenhua coal always suffer severe ash deposition problems.The experiment was done in a 0.25MW combustion facility to research contrastively the ash deposition process of two typical coals which have high and low deposition propensity respectively.For deposits sampled at different locations in the furnace burning Shenhua coal,the SEM(SED) and XRD techniques were used to identify the morphology and mineralogy characteristics respectively.Combined with the results provided by the probe measuring the heat flux in the furnace,a couple indices,viz.shedding periodicity of the deposition Tshed and the decaying amplitude of the heat flux Aq,were given to quantificationally evaluate the deposition propensity of different coals.The experiment results show that these quantificational indices can give good evaluation.The Tsh and Aq of Shenhua coal wich has high deposition propensity are Tsh 270min and Aq 92.7kW/m2 respectively,and for the low deposition propensity Xinwen coal,these indices are Tsh 58.5min and Aq23.77kW/m2.The mode of occurrence of iron and the transformation mechanism of iron minerals in Shenhua coal,which has high iron content,were disused based on the experimental results,and conclusion has been drawn that the silicate iron mineral particles contributes largely to the ash deposition process.
What problem does this paper attempt to address?