Toughening Mechanisms and Interfacial Bonding of W-ZrC Composites

Li Pengfei,Fan Jinglian,Han Yong,Zhang Man,Tian Jiamin
2019-01-01
Rare Metal Materials and Engineering
Abstract:W-ZrC composites are promising materials for plasma face components. In this paper, the W-ZrC composites were prepared by the method of "sol gel heterogeneous precipitation spray drying hydrogen reduction ordinary consolidation sintering". The toughening mechanisms and interfacial bonding of the W-ZrC composites were studied. The results show that ZrC particles can improve the strength and toughness of tungsten. The relative density and tensile strength of W-0.5wt%ZrC were 99.2% and 460 MPa, respectively after sintering at 1920 degrees C. Preliminary transient high-heat flux test shows that the W-ZrC composites can endure high-heat flux of 200 MW/m(2) (5 ms). ZrC particles have a process of growing up and rounding, and translate into nearly spherical particles when sintering at 1600 degrees C for 1 h. At the interfacial bonding zone of ZrC particles and tungsten, W, Zr, and C elements exhibit a smooth transition. The hardness of W, ZrC and interfacial bonging zone are 12, 22, and 18 GPa, respectively. SEM-EDS element line scanning and nanoindentation results indicate that the W and ZrC particles form (W, Zr)C compound.
What problem does this paper attempt to address?