Research on wrinkling behavior in tube hydroforming

XS Wang,SJ Yuan,ZR Wang
DOI: https://doi.org/10.3321/j.issn:0412-1961.2003.12.010
IF: 1.797
2003-01-01
ACTA METALLURGICA SINICA
Abstract:The common defects in tube hydroforming are buckling, wrinkling, bursting and folding. Wrinkling occuring as the axial force reaches a critical value is considered as one of defects in the past. Theoretical analyses, numerical simulation and experiment were conducted to control and use wrinkles in tube hydroforming. Effects of loading path and the ratio of length to diameter on the number of wrinkles and forming result were discussed. It has been shown that not all wrinkles are defects and tube can successfully be formed after wrinkling in some cases. The key issue is to obtain useful wrinkles instead of dead wrinkles. However, the thickness distribution is not even in the axial direction. Accumulation of material in the expanding area by formation of wrinkles is an effective method for preform. By use of this method, the zone of process window can be enlarged for hydroforming.
What problem does this paper attempt to address?