Analysis on Corner Wrinkling for Axial Hydro-Forging of Variable-Diameter Tube

Chu Guannan,Wang Qingfeng,Zhu Mingjing,Sun Lei,Ling Chen,Liu Xiehan
DOI: https://doi.org/10.1007/s00170-022-10783-2
2023-01-01
Abstract:Axial hydro-forging process is a promising alternative for the forming of variable-diameter tubes, in which the tube is subjected to bending and compression deformation. Consequently, wrinkling becomes the primary defects. Based on the corner wrinkling phenomena in corner filling stage of axial hydro-forging process, an analytical model was established to investigate the mechanism of the corner wrinkling and calculate the critical pressure. Subsequently, experiments and numerical analysis for axial hydro-forging were carried out. The effects of initial corner radius, thickness, and friction coefficient on critical pressure were investigated. It is found that the critical pressure decreases with increasing of the initial corner radius, but increases with increasing of the thickness. Through the analytical model, the critical loading path was obtained and compared with the experiments. The results validate that corner wrinkle can be suppressed when the internal pressure is above the critical pressure; otherwise, wrinkle occurs. It also indicates that the proposed analytical model is of practical significance for the hydro-forging process.
What problem does this paper attempt to address?