Microstructure and Shear Strength of ZrB2-SiC/Ti-6Al-4V Joint by TiCuZrNi with Cu Foam

Gang Wang,Zhentao Wang,Wei Wang,Rujie He,Kaixuan Gui,Caiwang Tan,Wei Cao
DOI: https://doi.org/10.1016/j.ceramint.2019.02.074
IF: 5.532
2019-01-01
Ceramics International
Abstract:In this paper, brazing behaviors between ZrB2-SiC and Ti-6Al-4V by Cu foam interlayer were studied. The microstructure, formation mechanism, mechanical property and fracture surface of the joints were systematically studied. The results showed that the phases in the joints were alpha + beta-Ti, TiCu, Ti2Cu, Cu(s, s), TiC, TiB2 and Ti3SiC2. An optimum shear strength reached up to 435 MPa at a brazing temperature of 910 degrees C and holding time of 20 min. Such a shear strength was 90 MPa higher than the one without the Cu foam. The obtained high shear strength of joint was discussed from microstructure and residual stress. With the increase of brazing time, Cu(s,s) gradually disappeared and the content of Ti2Cu intermetallic compound increased, which was harmful for the joint. Furthermore, the residual stress of joint with Cu foam was calculated to be 324 MPa, lower than the one without Cu foam interlayer.
What problem does this paper attempt to address?