Microstructural characterization and mechanical properties of ZTA/ZTA joint brazed by Ni50Ti50 filler metal

Kaihong Zheng,Qi Zhang,Juan Wang,Yao Lu
DOI: https://doi.org/10.1016/j.ceramint.2020.09.129
IF: 5.532
2021-01-01
Ceramics International
Abstract:<p>Obtaining reliable zirconia-toughened alumina (ZTA) ceramics brazed joints is highly crucial for expanding their applications. ZTA ceramics were successfully brazed with Ni<sub>50</sub>Ti<sub>50</sub> active filler metals. The interfacial microstructure of ZTA/Ni–Ti/ZTA joints was characterised through SEM, EDS, XRD and Raman spectroscopy. The effects of holding time on the microstructure and shear strength of the joints were investigated. During brazing, both Al<sub>2</sub>O<sub>3</sub> and ZrO<sub>2</sub> reacted with the Ni<sub>50</sub>Ti<sub>50</sub> filler and formed a AlNi<sub>2</sub>Ti + Ni<sub>2</sub>Ti<sub>4</sub>O double layer at the interface. ZrO<sub>2</sub> involved in the interfacial reaction transformed into oxygen-deficient ZrO<sub>2-x</sub>, and ZrO<sub>2-x</sub> particles were present in the reaction layer because of Al<sub>2</sub>O<sub>3</sub> consumption. NiTi and Ni<sub>3</sub>Ti compounds precipitated at the centre of a brazing seam. With an increase in the holding time, the thickness of AlNi<sub>2</sub>Ti and Ni<sub>2</sub>Ti<sub>4</sub>O gradually increased and more ZrO<sub>2-x</sub> particles appeared in the reaction layer. The mechanisms of interfacial microstructure formation and evolution were proposed. The maximum shear strength of 138 MPa was obtained for ZTA brazed at 1320 °C for 45 min. Nano-indentation was conducted to characterize the hardness, elastic modulus and plastic deformability of the reaction products, in order to analyse the fracture mechanism of the joints.</p>
materials science, ceramics
What problem does this paper attempt to address?