Amorphous silicoboron carbonitride monoliths resistant to flowing air up to 1800 °C

Bin Liang,Zhi-Hua Yang,De-Chang Jia,Jian-Cun Rao,Dong-Li Yu,Yong-Jun Tian,Quan Li,Yang Miao,Qi-Shuai Zhu,Yu Zhou
DOI: https://doi.org/10.1016/j.corsci.2016.03.026
IF: 7.72
2016-01-01
Corrosion Science
Abstract:TEM images showing the microstructure and morphologies of a cross section of oxidized SiBCN ceramic sample at 1700°C for 8h. (a) BF image showing the morphologies on the cross section; (b)–(d) BF images at high magnification corresponding to the zones marked by boxes B, C and D in (a), respectively; (e) SAED pattern corresponding to the zones marked by the circle E in (a); (f)–(g) HRTEM images corresponding to the zone marked by the circle F&G in (a); (h) linear scanning result showing the element distribution along the red line H in (a).
What problem does this paper attempt to address?