Abstract:In this investigation, TiN-reinforced W–Ti alloys were fabricated through spark plasma sintering of milled TiH2 powders and micro-sized W powders. TiH2 powder was used to prevent oxidation during milling. X-ray, FESEM, and TEM analyses were adopted to study the microstructures of the powders and sintered samples. As the Ti content increased from 0wt.% to 4wt.%, the grain size of the resultant alloy was significantly refined and a more transgranular fracture was observed. The micro-hardness of the alloys significantly increased with addition of up to 4wt.% Ti and then decreased with further Ti addition. A Ti/TiN solution in which N probably diffused into other Ti lattices during the sintering process was detected by TEM. The effect of He+ irradiation was investigated in this work. Samples with 0 and 8wt.% Ti were exposed to a He+ ion beam (He+ ion beam flux, 1.2×1022ions/m2·s; beam energy, 50eV) for 1h through the Large-Power Materials Irradiation Experiment System. Results revealed peeling off of TiN particles after irradiation as well as the presence of pores that could induce erosion in the grain boundaries. The sample with 8wt.% Ti showed no secondary-phase peeling, and only a small density of blisters were found in its W-grain and Ti-rich phases.
What problem does this paper attempt to address?