Preparation of TiC-doped W-Ti Alloy and Heat Flux Performance Test under Laser Beam Facility

Jing Shi,Lai-Ma Luo,Shuang Wang,Wei-Qi Pan,Qiu Xu,Xiang Zan,Xiao-Yong Zhu,Ji-Gui Cheng,Yu-Cheng Wu
DOI: https://doi.org/10.1016/j.fusengdes.2017.11.026
IF: 1.905
2018-01-01
Fusion Engineering and Design
Abstract:TiC-doped W-Ti composites were prepared by mechanical alloying and spark plasma sintering. The influence of milling time on the microstructure and properties of TiC-doped W-Ti composite material was investigated. Results show that with increasing ball milling time, powder particles undergo a process of fracture-cold welding fracture. Powder grains are continuously refined to 25.1 nm, and micro-strain continuously increases from 0.324% to 0.724%. With the extension of ball milling time, the sintered composite material exhibits a declining trend in density and an initial decrease and later increase in grain size. The minimum grain size is noted in the specimen WTT-60 at 0.35 mu m. Microhardness increases first then decreases, and the microhardness of specimen VVTT-60 reaches the highest value (1139.27 Hv) among those tested. Heat-shock resistance of the specimens was researched though a transient heat load experiment at pulse width 1 ms, current 60 A, and laser beam spot diameter 0.6 mm (44 similar to 47 MW/m(2)).The bulk prepared by powder sintering from 60 h of ball milling presents the best thermal shock resistance.
What problem does this paper attempt to address?