Preparation of Li7P3S11 Glass-Ceramic Electrolyte by Dissolution-Evaporation Method for All-Solid-state Lithium Ion Batteries

R. C. Xu,X. H. Xia,Z. J. Yao,X. L. Wang,C. D. Gu,J. P. Tu
DOI: https://doi.org/10.1016/j.electacta.2016.09.155
IF: 6.6
2016-01-01
Electrochimica Acta
Abstract:Design/fabrication of solid state electrolytes with high ionic conductivity is of great importance to develop next-generation Li ion batteries. In this work, the Li7P3S11 glass-ceramic electrolyte is successfully synthesized by dissolution- evaporation approach. The solvent effect on the electrochemical performance of Li7P3S11 is investigated by electrochemical impedance spectroscopy and chronoamperometry tests. The Li7P3S11 electrolyte prepared by a solution of acetonitrile has a high ionic conductivity of 9.7×10−4Scm−1 at 298K and a low activation energy of 31.2kJmol−1. Impressively, a wide and stable electrochemical window up to 5V (vs. Li/Li+) is demonstrated between the solid electrolyte and lithium electrode. The developed dissolution-evaporation approach shows good industrial prospect due to its advantages of energy conservation and high efficiency.
What problem does this paper attempt to address?