Strong Interfacial Adhesion between the Li 2 S Cathode and a Functional Li 7 P 2.9 Ce 0.2 S 10.9 Cl 0.3 Solid-State Electrolyte Endowed Long-Term Cycle Stability to All-Solid-State Lithium–Sulfur Batteries

Lei Zhou,Muhammad Khurram Tufail,Niaz Ahmad,Tinglu Song,Renjie Chen,Wen Yang
DOI: https://doi.org/10.1021/acsami.1c06328
2021-06-14
Abstract:The extrinsic cathode interface between the sulfide electrolyte and the Li<sub>2</sub>S electrode is always ignored in all-solid-state lithium–sulfur batteries. However, the aggregation of the Li<sub>2</sub>S cathode is still observed during cycling. The gradually lost extrinsic contact interface between the cathode and the electrolyte would result in considerable interface resistance and severe capacity decay in the cell due to the lack of efficient electron and ionic conduction at the interface. Herein, a facile dual-doping strategy demonstrates the synthesis of a functional inorganic electrolyte. The obtained Li<sub>7</sub>P<sub>2.9</sub>Ce<sub>0.2</sub>S<sub>10.9</sub>Cl<sub>0.3</sub> glass–ceramic electrolyte shows a higher-lithium-ionic conductivity of 3.2 mS cm<sup>–1</sup> at room temperature. Further, UV–vis absorption and ex situ scanning electron microscopy studies confirm robust interfacial adhesion between the functional inorganic electrolyte, Li<sub>7</sub>P<sub>2.9</sub>Ce<sub>0.2</sub>S<sub>10.9</sub>Cl<sub>0.3</sub>, and the Li<sub>2</sub>S cathode. Thus, a stable extrinsic cathode interface is unprecedently built. Finally, the all-solid-state lithium–sulfur battery based on the Li<sub>7</sub>P<sub>2.9</sub>Ce<sub>0.2</sub>S<sub>10.9</sub>Cl<sub>0.3</sub> electrolyte delivers a higher reversible initial capacity of 617 mA h g<sup>–1</sup>, a lower interface resistance of 25 Ω cm<sup>2</sup> and much better cycling stability (with a high capacity retention of 89% after 100 cycles) than the pristine Li<sub>7</sub>P<sub>3</sub>S<sub>11</sub> electrolyte.The Supporting Information is available free of charge at <a class="ext-link" href="/doi/10.1021/acsami.1c06328?goto=supporting-info">https://pubs.acs.org/doi/10.1021/acsami.1c06328</a>.XPS spectra of the Li<sub>7</sub>P<sub>3</sub>S<sub>11</sub>, Li<sub>7</sub>P<sub>2.9</sub>Ce<sub>0.2</sub>S<sub>11.1</sub>, and Li<sub>7</sub>P<sub>2.9</sub>Ce<sub>0.2</sub>S<sub>10.9</sub>Cl<sub>0.3</sub> glass–ceramic samples; TOF-SIMS spectra of the Li<sub>7</sub>P<sub>3</sub>S<sub>11</sub> glass–ceramic sample; morphology and microstructure of Li<sub>7</sub>P<sub>3</sub>S<sub>11</sub> glass–ceramic; morphology and microstructure of Li<sub>7</sub>P<sub>2.9</sub>Ce<sub>0.2</sub>S<sub>10.9</sub>Cl<sub>0.3</sub> glass–ceramic; electrochemical stability window between 2 and 5 V for the Li<sub>7</sub>P<sub>2.9</sub>Ce<sub>0.2</sub>S<sub>10.9</sub>Cl<sub>0.3</sub> glass–ceramic electrolyte; schematic diagram of the all-solid-state Li–S battery based on the Li<sub>2</sub>S composite cathode; Li<sub>2</sub>S solution, Li<sub>7</sub>P<sub>3</sub>S<sub>11</sub> glass–ceramic sample in Li<sub>2</sub>S solution, and Li<sub>7</sub>P<sub>2.9</sub>Ce<sub>0.2</sub>S<sub>10.9</sub>Cl<sub>0.3</sub> glass–ceramic sample in Li<sub>2</sub>S solution before static adsorption (<a class="ext-link" href="/doi/suppl/10.1021/acsami.1c06328/suppl_file/am1c06328_si_001.pdf">PDF</a>)This article has not yet been cited by other publications.
materials science, multidisciplinary,nanoscience & nanotechnology
What problem does this paper attempt to address?