Rapid Bonding of Ti3SiC2 and Ti3AlC2 by Pulsed Electrical Current Heating

Lu Shen,Jianming Xue,Michel W. Barsoum,Qing Huang
DOI: https://doi.org/10.1111/jace.13323
IF: 4.186
2014-01-01
Journal of the American Ceramic Society
Abstract:Inspired by pressure resistance welding of metallic materials, herein we describe how two MAX phases—Ti3SiC2 and Ti3AlC2—were successfully joined by a rapid electric current heating method in a pulsed electric current sintering furnace. No welding agent was employed and the total processing time was less than 6 min. When the bulk temperature of the joint couple exceeded 1070°C, good joints, with shear strength above 50 MPa, were achieved in both homo‐ and heterojunction joints.