Effect of SiC Nanowires on the Thermal Shock Resistance of Joint Between Carbon/carbon Composites and Li2O–Al2O3–SiO2 Glass Ceramics

Qian-Gang Fu,Han Peng,Xiao-Ying Nan,He-Jun Li,Yan-Hui Chu
DOI: https://doi.org/10.1016/j.jeurceramsoc.2014.03.011
IF: 5.7
2014-01-01
Journal of the European Ceramic Society
Abstract:In order to improve the bonding property of joint between SiC modified carbon/carbon (C/C) composites and Li2O–Al2O3–SiO2 (LAS) glass ceramics, SiC nanowires were attempted as the reinforcement materials in the interface region of SiC transition layer and Li2O–MgO–Al2O3–SiO2 (LMAS) gradient joining interlayer. The C/C–LAS joint with SiC nanowire-reinforced interface layer was prepared by a three-step technique of pack cementation, in situ reaction and hot-pressing. The microstructure and thermal shock resistance of the as-prepared joints were examined. The average shear strength of the joined samples with SiC nanowires increased from 24.9MPa to 31.6MPa after 40 thermal cycles between 1000°C and room temperature, while that of the joined samples without SiC nanowires dropped from 21.4MPa to 8.3MPa. The increase of thermal shock resistance of the C/C–LAS joints was mainly attributed to the toughening mechanism of SiC nanowires by pullout, bridging and crack deflection.
What problem does this paper attempt to address?