Abstract:In the NiAl alloys doped with 0.10 and 0.30 Sc (mass fraction, %) a Sc - rich second phase precipitated, but no Sc - rich phase was formed in the NiAl - 28Cr - 6Mo eutectic alloys doped with the same Sc contents. This difference is related with the expansion of the solid solubility of Sc in beta phase of the eutectic alloys. From the ambient temperature to high temperature (1373 K), the strength of NiAl alloys increased with increasing Sc content because of the substitutional solid solution strengthening of Sc element and Sc - rich second phase strengthening. The strengthening trend of the eutectic alloys at room temperature was the same as that of NiAl alloy, however, the influences of Sc on strength of the alloys at high temperature are negligible, which is the results of the absence of Sc - rich phase and weakening of solid solution strengthening at high temperature.
What problem does this paper attempt to address?