Microstructures and mechanical properties of high-silicon aluminum alloy fabricated by rapid solidification/powder metallurgy

杨伏良,甘卫平,陈招科,刘泓
DOI: https://doi.org/10.3321/j.issn:1004-0609.2004.10.017
2004-01-01
Abstract:Hypereutectic high-silicon aluminum alloy (Al-30Si and Al-40Si) was fabricated with a method in which air-atomization was followed by vacuum canning hot-extrusion process. Microstructure was analyzed by SEM and optical microscopy; tensile strength was examined and discussed. Experimental results show that, powder particle size is approximately 2-10 μm; silicon crystals are fine and uniform distributed by extrusion. The tensile strength reaches 239 MPa at 370°C extrusion, increases 77% compared with as cast, while tensile strength decreases, Si crystal grows up with both the extrusion temperature and the Si content increasing.