Fabrication and Mechanical Behaviors of 2D C/SiC–BC X Composite at Room Temperature

Yongsheng Liu,Laifei Cheng,Litong Zhang,Wenbin Yang,Shengtian Zhou,Weihua Zhang
DOI: https://doi.org/10.1177/0021998311417644
IF: 3.191
2011-01-01
Journal of Composite Materials
Abstract:C/SiC composite modified with boron carbide (BC x) matrix (entitled: C/SiC–BC x composite) was fabricated by chemical vapor infiltration (CVI). The densification behavior, microstructure, and mechanical behaviors of C/SiC–BC x composite were investigated. The results indicated that the density increase, corresponding with a decreasing porosity when CVI times increase. The density achieves 2.2 g cm−3 with 5% open porosity ratio. Inner fiber bundle, the matrix is SiC. Among fiber bundles, the matrices are composed with multilayer SiC and BC x. The non-brittle flexural fracture behavior was demonstrated and the flexural strength is 442 MPa. The fracture toughness is 22.84 MPa.m1/2. The non-linear tensile behavior was also demonstrated and the strength is 250 MPa. The compressive curve of sample is linear and the strength is 280 MPa. The in-plane shear behavior is also non-linear and shear strength is 160.9 MPa. The inter-laminar shear behavior is linear and the shear strength is 32.5 MPa. All mechanical behaviors of 2D of the C/SiC–BC x composite have been compared with that of the C/SiC composite.
What problem does this paper attempt to address?