Abstract:The effect of SiC on the oxidation performance of Zr-2[Al(Si)](4)C-5-SiC composites at 1000-1300 degrees C was explored. The present results demonstrated that scale growth on Zr-2[Al(Si)](4)C-5 ceramics obeyed a nearly linear rate law during oxidation, while the oxidation rate of Zr-2[Al(Si)](4)C-5-20SiC ceramics obeyed a nearly parabolic law, increasing rapidly during the initial stages of the reaction and then becoming slower. The oxidation resistance of Zr-2[Al(Si)](4)C-5-20SiC was improved remarkably: this was likely due to the formation of more protective oxide scales on the ceramic consisting of viscid aluminosilicate glass. (C) 2011 Elsevier Ltd. All rights reserved.