Barium titanate derived from mechanochemically activated powders

L.B Kong,J Ma,H Huang,R.F Zhang,W.X Que
DOI: https://doi.org/10.1016/S0925-8388(01)01925-9
IF: 6.2
2002-01-01
Journal of Alloys and Compounds
Abstract:A high-energy ball milling process was applied to a mixture with equal molar ratio of BaCO3 and TiO2. X-ray diffraction data indicated that there was no reaction happening during the milling process although the particle size was greatly reduced. The effect of post-annealing on the phase formation and grain growth of BaTiO3 was investigated by thermal analysis (DTA/TGA), X-ray diffraction (XRD) and scanning electron microscopy (SEM). No reaction was observed in the sample annealed at 600°C. Ba2TiO4 was found as the mixture annealed at 700°C. An 800°C-annealing led to single phase BaTiO3 with a cubic structure. The temperature at which BaTiO3 phase was derived is lower than required by the solid-state reaction process, which could be attributed to the refined grains/particles of the mixture as a result of high-energy ball milling. Tetragonal structured BaTiO3 was formed at 1150°C together with a sharp increase in grain size.
What problem does this paper attempt to address?