Study on the formation mechanism of Y-Ti-O oxides during mechanical milling and annealing treatment

Jiarong Zhang,Yanfen Li,Feiyang Bao,Xiang Rui,Zhengang Duan,Wei Yan,Quanqiang Shi,Wei Wang,Yiyin Shan,Ke Yang
DOI: https://doi.org/10.1016/j.apt.2021.01.005
IF: 4.969
2021-02-01
Advanced Powder Technology
Abstract:<p>Y-Ti-O nano-scale oxides play important roles in ensuring the excellent performance of oxide dispersion strengthened (ODS) steels. In this study, a model powder system of Y<sub>2</sub>O<sub>3</sub> and Ti was designed to investigate the formation and evolution mechanism of Y-Ti-O oxides. The morphology of powders tended to be stable after high energy ball milling for 240 min in Ar. X-ray diffraction (XRD) results suggested that there was no formation of new phase after mechanical milling. Thermo-gravimetric and differential thermal analysis (TG-DTA) was applied to analyze physical and chemical reactions of milled powders respectively in Ar and air. The corresponding annealing and XRD were performed to study the types and structures of oxides at different temperatures. It shows that oxygen concentration and temperature are the critical factors affecting the formation of oxides. Ti was evolved into Ti<sub>6</sub>O, Ti<sub>3</sub>O and TiO<sub>2</sub> in turn with temperature increasing. Then only TiO<sub>2</sub> was reacted with Y<sub>2</sub>O<sub>3</sub> to form Y<sub>2</sub>Ti<sub>2</sub>O<sub>7</sub>. The formation of Y<sub>2</sub>Ti<sub>2</sub>O<sub>7</sub> began at around 500 ℃ and was completed around 1004 ℃. A maximum formation rate occurred at about 779 ℃. High resolution transmission electron microscopy (HRTEM) suggested that the main phase in powders sintered at 1100 ℃ was identified as pyrochlore structure Y<sub>2</sub>Ti<sub>2</sub>O<sub>7</sub>.</p>
engineering, chemical
What problem does this paper attempt to address?